Loading Port:Xiamen
Payment Terms:TT OR LC
Min Order Qty:3 m.t.
Supply Capability:500 m.t./month
Appearance ( color ) | : light white transparent liquid | |
2 | Solid content(NV%) | : 6.3±0.2% |
3 | Viscosity | :27s±2s |
4 | Diluent | : water |
washing solvent | ||
5 | Coating solution temp. | : normal temperature |
6 | Storage condition | : 5~30°C |
7 | WVTR result | :NOT AVAILABLE |
8 | O2TR result | :≤75px3/m2•24h•0.1MPa |
9 | Compatibilityand good bond coating with polyurethane adhesive | Enough |
: polyesther or polyether adhesive | ||
10 | Appearance after coating | : ( must brightly or clearly |
11 | Bonding strength between PET and PVA | ………………………………gr/15mm or N/15mm |
We have organized several common questions for our clients,may help you sincerely:
①How about your company?
one of the largest thermal film manufactures in China. We are engaged in developing and producing new types of environmental friendly laminating materials(thermal laminating film for offset prints, digital prints and advertising inject prints).Our products are exported to Europe, North America, South America, South East Asia, etc.
②What is the package?
3 inch paper roll is always made with more than 1000 meters,so it is always packaging with one roll one carton.And 1 inch paper core is made with below 500meters,so we always packaging it with 9 rolls with one carton.and then by pallet.
③How to application manual?
.Adjust roller pressure and temperature according to different types of paper and ink.
.When using the film for the first time or changing to other sizes, we recommend a small trial volume before going into fully mass lamination.
.The following situation will affect the quality of the film during lamination.
a. When using metal ink
b. When the ink contains too much wax, dried oil, adhesive, and silicon additive. etc
c. When the ink is too thick
d. When the ink is not completely dry
e. When the paper contains too much moisture
f. When there is too much powder