Hot blast stove with low creep thermal shock high alumina brick

Loading Port:China Main Port

Payment Terms:TT OR LC

Min Order Qty:-

Supply Capability:-

Product Description:


       热风炉用低蠕变耐热震高铝砖

项目
item

HD

HS

HB

Al2O3 %

53

57

65

Fe2O3 %

1.7

0.8

0.8

TiO2 %

0.6

0.5

0.5

R2O %

0.6

0.6

0.6

显气孔率, %
A.P.

20

20

20

体积密度,g/cm3
B.D.

2.35

2.40

2.45

常温耐压强度,MPa
CCS

40

40

50

蠕变率,%(20—50h)
Creeping rate

0.2(1350)

0.2(1400)

0.2(1450)

重烧线变化,%(1400℃x4h)
P.L.C.

±0.2

±0.2

± 0.2

荷重软化温度0.5%,℃
RUL

135 0

1470

1520

抗震稳定性(1100℃,水冷)
Thermal shock(110o℃water)

20

20

20

Product features: hot blast stove with low creep heat shock high alumina brick using selected andalusite, sillimanite and corundum, mullite, high grade bauxite and flint clay as the main raw material, after high pressure forming, high temperature sintering. Products of low content of impurities, good thermal stability, high temperature creep performance is good, is the present domestic comprehensive type Dutch type hot blast stove technology to the characteristics and hot blast stove with refractory with Chinese characteristics.