Bitumen Modifier for Waterproofing Membrane

Loading Port:China Main Port

Payment Terms:TT or L/C

Min Order Qty:1*20'FCL m²

Supply Capability:10000 Tons per Year m²/month

Product Description:

 

 

Bitumen Modifier generally use a traditional waterproofing medium -- asphalt -- modified with atactic polypropylene (APP), styrene butadiene styrene (SBS), synthetic rubber or other agents that create a uniform matrix that enhances the physical properties of the asphalt.

 

 

 

 

Technical Data of Bitumen Modifier:

 

 

Item

S/B

Voliatility

≤%

Total Ash

≤%

Stress at 300%

(≥MPa)

Tensile strenth

≥MPa

Elongation

At break

(≥%)

Permanent

Deformation

(≥MPa)

Hardness shore (A)

Melt flow Index

(g/10min)

Main

application

1301-1

30/70

0.70

0.20

2.2

16

700

40

68

0.5-2.5

Bitumen

modification

4303

30/70

0.50

0.02

2.5

11

590

12

80

-

Bitumen

modification

2303

30/70

1.00

0.20

1.7

12

650

40

75

-

Bitumen

modification

511

30/70

0.60

1.0

-

-

-

-

75

0.5

Bitumen

modification

5301

31/69

0.40

1.0

-

-

-

-

74

0.5

Bitumen

modification

5300

40/60

0.40

0.20

-

-

-

-

88

8-10

Bitumen

modification

F501

31/69

0.75

-

-

13

650

-

≥70

≤1.0

Bitumen

modification

Adhesive

 

 

 

Properties of Bitumen Modifier:

 

Appearance of white or yellowish porous particles of rod or wafer shape. It process the advantages of both rubber and plastic with excellent low temperature endurance, ventilatiing and wet-and-slipping resistance.