Loading Port:Qingdao
Payment Terms:TT OR LC
Min Order Qty:5000 m²
Supply Capability:2000000 m²/month
Description
HDPE geomembrane are made from High density polyethylene polymer by bolw film process .
Have Smooth surface , Textured surface , Anti-Skid suface
HDPE Geomembrane Main Function
Antiseepage and seperation
Geomembrane Property
1. Good flexibility
2. For service temperature range : -70℃ ~ +110℃
3. Corrosion resistance , aging resistance
4. Excellent environmental stress cracking resistance property
5. High tensile strength and elongation
HDPE Geomembrane Usage
Landfills , sewage or waste treatment seeage .
River bank , lake dam , dam , water dam and reservoir, channel , has liquid pool ( pit , mine )
Metro , basements and tunnels , tunnel seepage control lining Foundation and other foundation saline seepage
Embankment , upstream impervious blanket level , foundation vertical impermeable layer , cofferdam construction , waste disposal
Sea water , fresh water fish farm
Road , highway , railway foundation expansive soil and loess of the waterproof layer
Roof impervious
HDPE Geomembrane Specification
No. | Item | Test Value | |||||||||
0.75mm | 1.0 mm | 1.25 mm | 1.5 mm | 2.0 mm | 2.5 mm | 3.0mm | |||||
1 | Minimum Density(g/cm³) | 0.939 | |||||||||
2 | Tensile Property | ||||||||||
Yield Strength ,N/mm | 11 | 15 | 18 | 22 | 29 | 37 | 44 | ||||
Break Strength ,N/mm | 20 | 27 | 33 | 40 | 53 | 67 | 80 | ||||
Yield Elongation ,% | 12 | ||||||||||
Break Elongation ,% | 700 | ||||||||||
3 | Tear Resistance N | 93 | 125 | 156 | 187 | 249 | 311 | 374 | |||
4 | Puncture Resistance N | 240 | 320 | 400 | 480 | 640 | 800 | 960 | |||
5 | Stress Crack Resistance, hrs | 300 | |||||||||
6
| Carbon Black | ||||||||||
Carbon Black Content, % | 2.0-3.0 | ||||||||||
Carbon Black Dispersion | Carbon black dispersion(only near spherical agglomerates) for 10 different views 9 in categories 1 or 2 and 1 in category 3 | ||||||||||
7
| Oxidative induction time(OIT) | ||||||||||
Standard OTI Min | 100 | ||||||||||
High Pressure OTI Min | 400 | ||||||||||
8 | Oven aging at 85℃ | ||||||||||
Standard OIT-% retained after 90 days | 55 | ||||||||||
High pressure OIT-% retained after 90 days | 80 | ||||||||||
9 | UV Resistance | ||||||||||
Standard OIT retained after 1600 hrs | 50 | ||||||||||
High pressure OIT retained after 1600 hrs | 50 | ||||||||||
10 | Low tempreture impact brittle property at -70°C | Pass | |||||||||
11 | Water vapor permeability (g.cm/cm2 .s.Pa) | ≤1.0×10-13 | |||||||||
12 | Dimensional Stability (%) | ±2 |
Gemembrane Show:
FAQ:
- Q1: Can you provide a sample for us?
A:Yes,We can send free samples,but customer need to pay the freight.
HDPE Geomembrane Price
- Q2: What is your minimum order quantity?
A:The minimum order quantity is 5000 ,but it is negotiable.
HDPE Geomembrane Price
- Q3:What is your payment terms?
A: T/T,Western Union,Paypal,L/C...
HDPE Geomembrane Price
- Q4:What is your delivery time?
A:Production time usually costs 2-20 days.