Glass Furnace Superstructures Refractory Block

Loading Port:Qingdao

Payment Terms:TT OR LC

Min Order Qty:500 m.t.

Supply Capability:1000 m.t./month

Product Description:

Features:

 

1. Strong glass corrosion resistance and high thermal shack stability.

 

2. Good RUL, wear-resistance, dregs-resistance and alkali corrosion resistance.

 

3. The products are adopting superior material, with process by special arc furnace forming it. This fused cast technology got nearly no suffer from electrode pollution. They can be widely used in the lining of glass furnace, the chemical industrials, metallurgical furnace.

  

Our company can produce serious specification fused cast 33#, 36#, 41#AZS block for glass furnace and its output is over 5000tons per year. In the enormous working premises—more than 6600square meters, there are one 5tons outside cooling electric arc furnace, high-power transformer, thaw craft with computer control system and internal advanced fused cast refractory umeral control grinding equipments according to its body producing ability.

 

Erosion-resistance to glass metal

 

Physical and chemical index of Fused Cast AZS41# for glass furnace

 

Item

Behaviors

AZS-33#

ER 1681

AZS-36#

ER 1685

AZS-41#

ER 1711

Chemical

Composition

Al2O3

≥50.00

≥49.00

≥45.00

ZrO2

≥32.50

≥35.50

≥40.50

SiO2

≤15.50

≤13.50

≤13.00

Na2O+K2O

≤1.30

≤1.35

≤1.30

Bulk density g/cm3

≥3.75

≥3.85

≥4.00

Apparent Porosity %

≤1.2

   ≤1.0

≤1.2

Cold Crushing Strength  Mpa

≥300

≥300

≥300

Exudation Temperature of Glass Phase

≥1400

≥1400

≥1410

Bubble Separation Ratio(1300°C×10h)

≤1.2

≤1.0

≤1.0

Anti-corrosion rate of glass liquid

1500°C×36h (mm/24h)%

≤1.4

≤1.3

≤1.2

Apparent density

(g/cm3)

PT(RN RC N)

≥3.50

≥3.50

≥3.70

ZWS(RR EVF EC ENC)

≥3.65

≥3.70

≥3.90

WS( RT VF EPIC FVP DCL)

≥3.75

≥3.8

≥4.00

         1.High purity

   Good self-sharpening

           Grinding ability