Product Description:

Powder JS waterproof material is a green waterproof material, the material is a composite of an organic binder and inorganic powder made of waterproof material, with a simple construction, low cost, good waterproof effect and so on.

usable range:

Based on the dry powder JS waterproof material may be wet or dry masonry, mortar, concrete, metal, wood, hard plastic, glass, gypsum board, foam board, asphalt, rubber, SBS membrane, APP membrane, polyurethane, etc. construction, industrial and civil construction of new 1st (example: houses, walls, underground, tunnels, bridges, ponds, reservoirs, bathroom, kitchen) can be used.

Directions:

* Primary surface smooth, solid, no sharp objects, dust and clear water, clean oil:

* Yang angle and pipes etc. should be made of the root of the arc-shaped, overcast corner radius greater than 25mm. Sun angle radius greater than 5mm;

* Must first leveling uneven and cracks, leaks must first plugging process.

Ingredients:

* The first increase in a barrel of water, with a mixer while stirring while slowly adding powder, stirring for 5 minutes, stirring until evenly substandard feed pellets, with a good material should be used within two hours, otherwise it will affect the viscosity increases construction;

 * The amount of water added can be appropriately adjusted in order to adjust the viscosity of the material, to meet the construction facades and different parts of the plane;

 * Fill in the groove seal material embedded in the yin and yang angle, root canal and other details should be many times (2-5 times) brushing, underground works should add a layer of carcass reinforcing material;

* Large-scale construction waterproof coating should be painted many times, usually three layers brushing, brushing special projects according to five layers:

  * Usually each brushing time interval of 8 hours to extend the winter, every time the film thickness of 0.4-0 5mm as well, again not too thick;

  * After the waterproof layer after completion of acceptance, coping finished product protection.